MIL-PRF-23827C
TABLE II. Qualification inspection and methods.
Requirements
Test method or paragraph
1/ ASTM-D4048
Corrosiveness (copper strip)
Dirt
FED-STD-791, Method 3005
ASTM-D2265
Dropping point
ASTM-D2595
Evaporation
FED-STD-791, Method335
Gear wear
ASTM-D3336
High temperature performance
Load carrying capacity
ASTM-D2596
Low temperature torque 2/
ASTM-D1478
Odor
4.5.1
Oil separation
ASTM-D6184
Oxidation stability
ASTM-D942
Penetration
ASTM-D217
Rust preventative properties
ASTM-D1743
Storage stability 3/
FED-STD-791, Method 3467
Water resistance
ASTM-D1264
Worked stability
FED-STD-791, Method 313
Visual
Workmanship
1/
The copper strip shall not tarnish more than a classification of 1b when compared with
ASTM copper strip corrosion standards. Test shall be conducted at 100° ±1°C for 24-hours.
2/
Test shall be conducted at -73° ±1°C. Observation for skidding or ball sliding shall be made
during test run.
3/
Temperature of 40° ±2°C to be maintained for 6 months.
6